Porcelain goblet. Dipped, slanted, into tenmoku (DMM4); dipped, slanted, into DMMH2; fine nibbed squirt of 11A (a white, with rutile – turns blue over the iron-based tenmoku). Inside: transparent 51. For glazes, thanks to Daniel de Montmollin, and Carol Youngner.
Fired to 1260°C, in oxidation.